Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 350 - 450 cP @Temperature 23.0 °C |
350 - 450 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Cast 200 3D Printing Polymer Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar. |
|||
Viscosity | 350 cP @Temperature 30.0 °C |
350 cP @Temperature 86.0 °F |
|
Proto3000 Accura® Amethyst™ Material for use with Viper™ SLA® systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. FEATURES:Outstanding accuracyExceptional detailHigh thermal resistanceDeep purple colorLow as.. |
|||
Viscosity | 350 - 450 cP | 350 - 450 cP | |
Huntsman CY 179 MA Multifunctional Resin Weight per Epoxide (EEW, g/eq) 131 to 143. Max color is 1.Comments/Applications: Alicyclic diepoxy carboxylate, low viscosity liquid epoxy. High temperature outdoor electrical and casting applicat.. |
|||
Viscosity | 350 cP @Temperature 25.0 °C |
350 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8026 Silicone Stabilizer for PU Foam STRUKSILON 8026 is used as a silicone stabilizer for the production of polyurethane shoe sole systems as well as other microcellular foams. It is especially recommended for shoe sole formulations ba.. |
|||
Viscosity | 350 - 700 cP | 350 - 700 cP | LVTDV-I-A3 V50; RP-0596 |
Solvay RHODOLINE® DF 540 Surfactant Description: Highly effective white oil defoamer for latex processing.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF 540 is a general purpose silicone-free, high a.. |
|||
Viscosity | 350 - 550 cP @Temperature 125 °C |
350 - 550 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® N-34 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-34 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Viscosity | 350 cP @Temperature 200 °C |
350 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3620 Polyester, Pellet High elongation type UE3215UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders,.. |
|||
Viscosity | 350 cP @Temperature 200 °C |
350 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3690 Polyester, Pellet High Tg, PET adhesiveness, High heat resistance, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as ad.. |
|||
Viscosity | 350 cP @Temperature 25.0 °C |
350 cP @Temperature 77.0 °F |
Mixed (sp #2, 10 rpm) |
Tra-Con Tra-Bond FS437 Low Viscosity High Impact Epoxy Adhesive TRA-BOND FS437 is a two-part, low viscosity material formulated for optical applications which require excellent wicking, visible color and high strength. This material has been used successfully fo.. |
|||
Viscosity | 350 cP | 350 cP | |
Dow Corning SYL-OFF® 7676 RELEASE COATING Syl-Off® 7676 Coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity hexenyl endblocked and pendant functional silicone polymer. Recommended for use against aggressiv.. |
|||
Viscosity | 350 cP | 350 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 200 Coating Low release at high speeds; high viscosityInformation provided by Dow Corning |
|||
Viscosity | 350 cP | 350 cP | dynamic |
Dow Corning SYL-OFF® SL 600 COATING Solvent-free, fast curing, provides extremely stable release, excellent bath stability, low release force across a variety of peel speeds, requires catalyst additionInformation provided by Dow Corni.. |
|||
Viscosity | 350 cP @Temperature 160 °C |
350 cP @Temperature 320 °F |
Melt; ETM 22-31 |
ExxonMobil ESCOREZ™ 5690 Petroleum Hydrocarbon Resin Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and polyolefins. Information provid.. |
|||
Viscosity | 350 cP @Temperature 30.0 °C |
350 cP @Temperature 86.0 °F |
|
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |
|||
Viscosity | 350 - 650 cP @Temperature 23.0 °C |
350 - 650 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Viscosity | 350 - 450 cP | 350 - 450 cP | |
Dow CYRACURE™ UVR-6110 Cycloaliphatic Epoxide CYRACURE™ UVR-6107 cycloaliphatic epoxide is a standard base resin. It is useful in many applications in which low viscosity is not required: Metal decoration coatings Overprint varnishes Informa.. |
|||
Viscosity | 350 - 500 cP @Temperature 35.0 °C |
350 - 500 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 90 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 350 cP | 350 cP | B Side |
ACC EP AJS EPI Engineered Polymers Aliphatic Joint Sealant EP AJS Aliphatic Joint Sealant, “Powered by Reactamine® Technology, is a two component 100% solid, aliphatic (silicone optional) polyurea based joint sealant. EP AJS is a self-leveling joint seala.. |
|||
Viscosity | 350 - 500 cP | 350 - 500 cP | |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 350 cP @Temperature 30.0 °C |
350 cP @Temperature 86.0 °F |
|
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing.. |
|||
Viscosity | 350 - 500 cP | 350 - 500 cP | blended |
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Viscosity | 350 cP | 350 cP | B Component; Spindle #2; speed 50 rpm; ASTM D1824 |
Aptek 6109-A/B Epoxy Encapsulant Optoelectronic grade flexible water clear encapsulant. Higher viscosity/lower Tg version for clear blob-top encapsulation of ceramic substrate devicesPart A is blue. Part B is clear to pale yellow.I.. |
|||
Viscosity | 350 cP @Temperature 200 °C |
350 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3600 Polyester, Pellet High Tg, PET adhesiveness, Transparency, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, .. |
|||
Viscosity | 350 cP @Temperature 40.0 °C |
350 cP @Temperature 104 °F |
Solution, 25% in Dimethylacetamide; Internal Method |
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU)
(Unverified Data**) Veradel A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t.. |