Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1500 cP | 1500 cP | |
Resinlab® CYNERGY CA6906 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Ritelok PR1500 Plastic & Rubber Adhesive Cyanoacrylate. Multi-purpose plastic & rubber adhesive. High strength bond & impact resistance. High bond strength, High viscosity, Excellent for gap filling |
|||
Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | |
ND Industries 542 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, fans, cams, collars, flywheels, rotors to shaftMeets military spec Mil-R-46082B Type III |
|||
Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
Uncured |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Resinlab® CYNERGY CA6010 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 1500 cP @Temperature 190 °C |
1500 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 1215 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance, short open time, and excellent wetting propertiesApplications: Lamination of reinforced tapes and prot.. |
|||
Viscosity | 1500 cP | 1500 cP | "B" component |
ACC QLE 1030 QSI Quantum Silicones 27 Durometer Addition Cure Elastomer for Coating
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: long pot life, excellent adhesion, 100%solid, fast cure.Applications: fabric or cloth coating. Part of the Amber Chem.. |
|||
Viscosity | 1500 - 4000 cP @Temperature 40.0 °C |
1500 - 4000 cP @Temperature 104 °F |
|
Taiwan PU Corporation PPG CPU-1060 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | #3 SP, 12 rpm; RP-1234 |
Solvay MIRACARE® MS-2 Surfactant Description: Formulated surfactant concentrate that is readily dilutable to yield ultra-mild cleansing products. Low eye and skin irritation.Chemical Name: AMPHOTERIC/ANIONIC/NONIONIC SURFACE ACTIVE.. |
|||
Viscosity | 1500 - 2000 cP | 1500 - 2000 cP | RP-0596 |
Solvay RHODOLINE® DF-988 Surfactant Description: Silicone free and mineral oil free defoamer for high gloss paints.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF-988 is a silicone-free, mineral oil-f.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Von Roll Isola IMI Varnish 74011 Solventless Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |
|||
Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond FDA8 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-8 EPOXY ADHESIVE is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food an.. |
|||
Viscosity | 1500 - 2500 cP @Temperature 23.0 °C |
1500 - 2500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7DC One Component, Dual Cure UV System Master Bond UV15-7DC is a one component, dual cure UV system for high performance bonding, sealing, coating and encapsulation applications. This system features a primary cure utilizing UV light and.. |
|||
Viscosity | 1500 cP @Temperature -20.0 °C |
1500 cP @Temperature -4.00 °F |
Cold Crank |
ChevronTexaco 5R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
|
Cytec (Conap) RN-1200 / EA-87 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
|
Cytec EN-13 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Viscosity | 1500 - 2500 cP @Temperature 23.0 °C |
1500 - 2500 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OE101 Two Component Epoxy Material Description: A two component epoxy designed for low stress applications in fiber optic packaging, opto-electronics and semiconductors. It is a lower modulus version of EPO-TEK® 353ND.Inf.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Dow ISONATE™ 240 MDI Prepolymer ISONATE™ 240 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with a high molecular weight polyester polyol, resulting in a material with good.. |
|||
Viscosity | 1500 cP | 1500 cP | dynamic |
Dow Corning 1520 SILICONE ANTIFOAM 20 percent active food-grade silicone emulsion that is water dilutable and effective in both hot and cold systems.Information provided by Dow Corning |
|||
Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | MA143LFE |
C.O.I.M. FILCO® 309 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Viscosity | 1500 cP | 1500 cP | After mixing, uncured |
Atom Adhesives AA-BOND FDA8 Epoxy Adhesive AA-BOND FDA8 EPOXY ADHESIVE is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and .. |
|||
Viscosity | 1500 cP | 1500 cP | |
Von Roll Isola IMI Varnish 704 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 42°C. Usag.. |
|||
Viscosity | 1500 cP | 1500 cP | Part B, RVT, #2, 20 rpm; TM R050-12 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Loctite® 415 General Purpose Methyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Loctite® 416 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 1500 - 3000 cP @Temperature 35.0 - 35.0 °C |
1500 - 3000 cP @Temperature 95.0 - 95.0 °F |
Average value: 2380 cP Grade Count:5 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |