Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.16e+6 cP | 1.16e+6 cP | Melt Viscosity, 240°C, 100 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® EX75 ABS Multi-purpose, extrusion ABS providing a favorable balance of engineering properties. |
|||
Viscosity | 1.16e+6 cP @Temperature 190 °C |
1.16e+6 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 5218 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, ethylene copolymer, and FDA compliantFeatures: High viscosity and high ring and ball softening pointApplications: Component .. |