Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.400 - 1.10e+6 cP | 0.400 - 1.10e+6 cP | Average value: 17700 cP Grade Count:373 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |