Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.0300 - 30000 cP | 0.0300 - 30000 cP | Average value: 5130 cP Grade Count:23 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |