Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.0 - 3.5 g/10 min | 1.0 - 3.5 g/10 min | I Preparation |
Sibur ABS 1106M Extrusion Grade ABS Plastic With high thermal and light resistance for production of sheets with following pneumatic and vacuum formation of internal parts for refrigerators and other articles of technical purpose. |
|||
Melt Index of Compound | 2.0 - 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 - 3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate LOTRYL® 29 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 29 MA 03 is a polyme.. |
|||
Melt Index of Compound | 2.5 - 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 - 3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 24-03 Copolymer Ethylene - Vinyl Acetate EVATANE® 24-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 24-03 is stabilized with antioxidants. The High Vinyl Acetate co.. |