Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 59 g/10 min @Load 5.00 kg, Temperature 190 °C |
59 g/10 min @Load 11.0 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® CA116-203 TPU-Polyester Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee.. |
|||
Melt Index of Compound | 59 g/10 min @Load 10.0 kg, Temperature 220 °C |
59 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall Information Provided by LG Chem |