Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 32 g/10 min @Load 2.16 kg, Temperature 250 °C |
32 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Index of Compound | 32 g/10 min @Load 5.00 kg, Temperature 300 °C |
32 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific) Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade. |
|||
Melt Index of Compound | 32 g/10 min @Load 5.00 kg, Temperature 280 °C |
32 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l.. |
|||
Melt Index of Compound | 32 - 37 g/10 min @Load 2.16 kg, Temperature 190 °C |
32 - 37 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 35 BA 320 Copolymer Ethylene - Butyl Acrylate LOTRYL® 35 BA 320 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 320 is particularly.. |
|||
Melt Index of Compound | 32 g/10 min @Load 10.0 kg, Temperature 280 °C |
32 g/10 min @Load 22.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has .. |