Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 23 g/10 min @Load 5.00 kg, Temperature 230 °C |
23 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs T00 ABS, Transparent Information provided by Polykemi AB |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1R PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount o.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1R PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific) CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Melt Index of Compound | 23 g/10 min @Load 3.80 kg, Temperature 230 °C |
23 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha.. |
|||
Melt Index of Compound | 23 g/10 min @Load 5.00 kg, Temperature 280 °C |
23 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
Melt Index of Compound | 23 g/10 min | 23 g/10 min | ASTM D1238 |
Cheng Yu Plastic 3255 TPE Rubber |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |