Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.10 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB SCANFILL BOTTLE BY45C2 Blow Molding Grade Information provided by Polykemi AB |
|||
Melt Index of Compound | 0.10 - 0.14 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.10 - 0.14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti.. |
|||
Melt Index of Compound | 0.10 - 0.14 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.10 - 0.14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac.. |
|||
Melt Index of Compound | 0.10 - 0.14 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.10 - 0.14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil.. |
|||
Melt Index of Compound | 0.10 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DGDB-2480 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in pipe applications where long term hydrostatic strength and resistance to slow crack growth are desired. Su.. |
|||
Melt Index of Compound | 0.10 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDB-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDB-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |