Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 3.17 mm |
0.0010 - 0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-68/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 1.00 mm |
0.0010 - 0.0020 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 1.00 mm |
0.0010 - 0.0020 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 1.00 mm |
0.0010 - 0.0020 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 1.00 mm |
0.0010 - 0.0020 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 3.17 mm |
0.0010 - 0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |