Linear Mold Shrinkage 0.018 cm/cm

@Thickness 3.20 mm
0.018 in/in

@Thickness 0.126 in
Parallel; DAM; ASTM D955
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.018 - 0.020 cm/cm

@Thickness 3.17 mm
0.018 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.018 - 0.022 cm/cm

@Thickness 6.35 mm
0.018 - 0.022 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.018 - 0.022 cm/cm

@Thickness 6.35 mm
0.018 - 0.022 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.018 - 0.023 cm/cm

@Thickness 3.00 mm
0.018 - 0.023 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-222SA Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.018 - 0.021 cm/cm

@Thickness 3.20 mm
0.018 - 0.021 in/in

@Thickness 0.126 in
Flow, 24h; ASTM D955