Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.000800 - 0.105 cm/cm | 0.000800 - 0.105 in/in | Average value: 0.00839 cm/cm Grade Count:221 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Linear Mold Shrinkage, Transverse | 0.0000300 - 0.105 cm/cm | 0.0000300 - 0.105 in/in | Average value: 0.00822 cm/cm Grade Count:114 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00530 - 0.105 cm/cm | 0.00530 - 0.105 in/in | Average value: 0.00969 cm/cm Grade Count:54 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage, Transverse | 0.0075 - 0.105 cm/cm | 0.0075 - 0.105 in/in | |
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Linear Mold Shrinkage, Transverse | 0.0075 - 0.105 cm/cm | 0.0075 - 0.105 in/in | |
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Linear Mold Shrinkage, Transverse | 0.00450 - 0.105 cm/cm | 0.00450 - 0.105 in/in | Average value: 0.00982 cm/cm Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |