Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0140 - 0.0250 cm/cm | 0.0140 - 0.0250 in/in | Average value: 0.0209 cm/cm Grade Count:5 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00122 - 0.0250 cm/cm | 0.00122 - 0.0250 in/in | Average value: 0.0164 cm/cm Grade Count:70 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0250 cm/cm | 0.00500 - 0.0250 in/in | Average value: 0.0145 cm/cm Grade Count:34 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |