Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0185 cm/cm | 0.0105 - 0.0185 in/in | Average value: 0.0131 cm/cm Grade Count:19 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage, Transverse | 0.0145 - 0.0185 cm/cm | 0.0145 - 0.0185 in/in | |
LATI Latigray 52/11-01 CX/45 PP Homopolymer Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0155 - 0.0185 cm/cm | 0.0155 - 0.0185 in/in | |
LATI Latistat 52/7-02 PP Homopolymer Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |