Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.000 - 0.0160 cm/cm
0.000 - 0.0160 in/in
Average value: 0.00900 cm/cm Grade Count:16
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage, Transverse 0.00160 - 0.0160 cm/cm
0.00160 - 0.0160 in/in
Average value: 0.00390 cm/cm Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0160 cm/cm
0.00100 - 0.0160 in/in
Average value: 0.00953 cm/cm Grade Count:32
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Linear Mold Shrinkage, Transverse 0.00600 - 0.0160 cm/cm
0.00600 - 0.0160 in/in
Average value: 0.00843 cm/cm Grade Count:14
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Linear Mold Shrinkage, Transverse 0.00150 - 0.0160 cm/cm
0.00150 - 0.0160 in/in
Average value: 0.00566 cm/cm Grade Count:137
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage, Transverse 0.000400 - 0.0160 cm/cm
0.000400 - 0.0160 in/in
Average value: 0.0103 cm/cm Grade Count:35
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage, Transverse 0.00250 - 0.0160 cm/cm
0.00250 - 0.0160 in/in
Average value: 0.00810 cm/cm Grade Count:28