Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0114 - 0.0130 cm/cm | 0.0114 - 0.0130 in/in | Average value: 0.0122 cm/cm Grade Count:4 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0130 cm/cm | 0.00500 - 0.0130 in/in | Average value: 0.00821 cm/cm Grade Count:37 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0130 cm/cm | 0.00700 - 0.0130 in/in | Average value: 0.00929 cm/cm Grade Count:14 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage, Transverse | 0.000 - 0.0130 cm/cm | 0.000 - 0.0130 in/in | Average value: 0.00702 cm/cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0130 cm/cm | 0.00200 - 0.0130 in/in | Average value: 0.00812 cm/cm Grade Count:47 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |