Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00200 - 0.00600 cm/cm
0.00200 - 0.00600 in/in
Average value: 0.00467 cm/cm Grade Count:3
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00600 cm/cm
0.00200 - 0.00600 in/in
Average value: 0.00333 cm/cm Grade Count:3
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Linear Mold Shrinkage, Transverse 0.00250 - 0.00600 cm/cm
0.00250 - 0.00600 in/in
Average value: 0.00456 cm/cm Grade Count:21
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Linear Mold Shrinkage, Transverse 0.00300 - 0.00600 cm/cm
0.00300 - 0.00600 in/in
Average value: 0.00410 cm/cm Grade Count:15
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Linear Mold Shrinkage, Transverse 0.00500 - 0.00600 cm/cm
0.00500 - 0.00600 in/in
Average value: 0.00550 cm/cm Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Linear Mold Shrinkage, Transverse 0.00600 - 0.00600 cm/cm

@Temperature 80.0 - 80.0 °C
0.00600 - 0.00600 in/in

@Temperature 176 - 176 °F
Average value: 0.00600 cm/cm Grade Count:6
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Linear Mold Shrinkage, Transverse 0.00450 - 0.00600 cm/cm
0.00450 - 0.00600 in/in
Average value: 0.00528 cm/cm Grade Count:3
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..