Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0124 cm/cm | 0.0124 in/in | |
Plastcom SLOVALEN PQ 81 T 10 PP, 10% mineral filling FeaturesModified PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Linear Mold Shrinkage, Transverse | 0.0124 cm/cm | 0.0124 in/in | STN 64 0808 |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Linear Mold Shrinkage, Transverse | 0.0124 cm/cm | 0.0124 in/in | |
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Linear Mold Shrinkage, Transverse | 0.0124 cm/cm @Thickness 2.00 mm |
0.0124 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**) Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P.. |
|||
Linear Mold Shrinkage, Transverse | 0.0124 cm/cm | 0.0124 in/in | ISO 294-4 |
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET
(Unverified Data**) Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like .. |
|||
Linear Mold Shrinkage, Transverse | 0.0124 cm/cm | 0.0124 in/in | 60x60x2 mm; ISO 294 |
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Linear Mold Shrinkage, Transverse | 0.0124 cm/cm | 0.0124 in/in | |
Plastcom SLOVALEN PQ 83 T 10 PP, 10% mineral filling FeaturesModified PP + EPDM for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal. Decreased shrinkage. Application in automotive, covers of car chas.. |
|||
Linear Mold Shrinkage, Transverse | 0.0124 cm/cm | 0.0124 in/in | |
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |