Polymer Property : Linear Mold Shrinkage, Transverse = 0.00800 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00800 - 0.00900 cm/cm
0.00800 - 0.00900 in/in
Average value: 0.00867 cm/cm Grade Count:3
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0400 cm/cm
0.00800 - 0.0400 in/in
Average value: 0.0140 cm/cm Grade Count:25
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0156 cm/cm
0.00800 - 0.0156 in/in
Average value: 0.0113 cm/cm Grade Count:5
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Linear Mold Shrinkage, Transverse 0.00800 - 0.00900 cm/cm
0.00800 - 0.00900 in/in
Average value: 0.00833 cm/cm Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0300 cm/cm
0.00800 - 0.0300 in/in
Average value: 0.0226 cm/cm Grade Count:6
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0302 cm/cm
0.00800 - 0.0302 in/in
Average value: 0.0171 cm/cm Grade Count:78
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0120 cm/cm
0.00800 - 0.0120 in/in
Average value: 0.0104 cm/cm Grade Count:5
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0230 cm/cm
0.00800 - 0.0230 in/in
Average value: 0.0148 cm/cm Grade Count:3
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0100 cm/cm

@Temperature 80.0 - 80.0 °C
0.00800 - 0.0100 in/in

@Temperature 176 - 176 °F
Average value: 0.00867 cm/cm Grade Count:3
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0200 cm/cm
0.00800 - 0.0200 in/in
Average value: 0.0169 cm/cm Grade Count:15
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0110 cm/cm
0.00800 - 0.0110 in/in
Average value: 0.00958 cm/cm Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..