Polymer Property : Linear Mold Shrinkage, Transverse = 0.0068 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0068 cm/cm
0.0068 in/in
Plastcom SLOVAMID 6 GF 60 000/1M PA6 reinforced with 60% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 60% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go..
Linear Mold Shrinkage, Transverse 0.0068 cm/cm
0.0068 in/in
STN 64 0808
Plastcom SLOVAMID 6 GF 60 Polyamide 6, 60% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 60% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Linear Mold Shrinkage, Transverse 0.0068 cm/cm
0.0068 in/in
60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Transverse 0.0068 cm/cm
0.0068 in/in
ASTM D955
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber
Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
Linear Mold Shrinkage, Transverse 0.0068 cm/cm

@Thickness 1.50 - 3.20 mm
0.0068 in/in

@Thickness 0.0591 - 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific)
LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry.
Linear Mold Shrinkage, Transverse 0.0068 cm/cm
0.0068 in/in
ISO 294-4
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Linear Mold Shrinkage, Transverse 0.0068 cm/cm
0.0068 in/in
ISO 294-4, 2577
Lanxess Durethan® DP AKV 35 LT H2.0 904040 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, black colored for laser transmission- welding (laser-transparent), good heat-ageing resistance