Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00122 - 0.0250 cm/cm | 0.00122 - 0.0250 in/in | Average value: 0.0164 cm/cm Grade Count:70 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00122 cm/cm | 0.00122 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP 2801 000000 Nylon 66 PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free |