Polymer Property : Linear Mold Shrinkage, Transverse = 0.00010 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse <= 0.00010 cm/cm

@Time 86400 sec
<= 0.00010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DEL139P PC
LNP* STAT-KON* DEL139P is a compound based on Polycarbonate containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: Electrically Conductive, Exceptional Processing, Flame Retar..
Linear Mold Shrinkage, Transverse 0.00010 cm/cm
0.00010 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide
Injection molding, reinforcedInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Transverse 0.00010 cm/cm
0.00010 in/in
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY
Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic..