Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.021 - 0.022 cm/cm | 0.021 - 0.022 in/in | ASTM D955 |
PolyOne Stat-Tech™ X ST6600-0041 ES NHFR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.022 cm/cm @Thickness 3.18 mm |
0.013 - 0.022 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® X PS-154200101 WHITE Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.022 cm/cm | 0.021 - 0.022 in/in | ASTM D955 |
PolyOne Stat-Tech™ NN-20SS/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.0195 - 0.022 cm/cm | 0.0195 - 0.022 in/in | |
LATI Latan 13 S/15 POM, 15% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.022 cm/cm @Thickness 3.20 mm |
0.020 - 0.022 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 305 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 1450-1850. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.022 cm/cm @Thickness 3.20 mm |
0.020 - 0.022 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 308 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.022 cm/cm @Thickness 3.20 mm |
0.020 - 0.022 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 309 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.022 cm/cm @Thickness 3.20 mm |
0.018 - 0.022 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LHI3 XE-NBK1 Impact Modified Engineering Nylon 66 Description: Impact Modified Engineering Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | DIS 294-4 |
Wellman Wellamid® 22LHI4 XE-GY1 Nylon 66, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | DIS 294-4 |
Wellman Wellamid® NY1875-BK1 Nylon 66, Unfilled All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | |
Solvay TECHNYL® 2210HS PA66, DRY Description: Polyamide 66, unfilled, long-term stabilized, lubricated for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 2210HS is used in all sectors of industry, offe.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LH-WBK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |