Polymer Property : Linear Mold Shrinkage, Transverse = 0.0185 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0105 - 0.0185 cm/cm
0.0105 - 0.0185 in/in
Average value: 0.0131 cm/cm Grade Count:19
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage, Transverse 0.0145 - 0.0185 cm/cm
0.0145 - 0.0185 in/in
LATI Latigray 52/11-01 CX/45 PP Homopolymer
Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Linear Mold Shrinkage, Transverse 0.0155 - 0.0185 cm/cm
0.0155 - 0.0185 in/in
LATI Latistat 52/7-02 PP Homopolymer
Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..