Linear Mold Shrinkage, Transverse 0.0145 - 0.0175 cm/cm
0.0145 - 0.0175 in/in
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant
Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Linear Mold Shrinkage, Transverse 0.0145 - 0.0175 cm/cm
0.0145 - 0.0175 in/in
LATI Latene® EP 7-V2 PP Copolymer, Flame Retardant
Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Linear Mold Shrinkage, Transverse 0.0145 - 0.0175 cm/cm
0.0145 - 0.0175 in/in
LATI Latiohm 52/11-10 PD02 PP Homopolymer
Dissipative product based on Polypropylene homopolymer (PPh). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..