Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0160 cm/cm | 0.0160 in/in | Average value: 0.0160 cm/cm Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage, Transverse | 0.0160 cm/cm | 0.0160 in/in | Average value: 0.0160 cm/cm Grade Count:4 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0160 - 0.0260 cm/cm | 0.0160 - 0.0260 in/in | Average value: 0.0211 cm/cm Grade Count:6 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |