Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0094 cm/cm | 0.0094 in/in | 60x60x2; 300°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0094 cm/cm | 0.0094 in/in | ISO DIS 294-4 |
Wellman EcoLon® MRGF1518-BK3 38% Mineral/Glass Reinforced Post Consumer Compound Nylon 66 Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0094 cm/cm | 0.0094 in/in | ISO Data |
BASF Ultradur B 4406 G6 Q113 30% Glass Filled PBT Ultradur B4406 G6 Q113 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |