Polymer Property : Viscosity = 349000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 349000 cP

@Shear Rate 500 1/s,
Temperature 215 °C
349000 cP

@Shear Rate 500 1/s,
Temperature 419 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)  (Unverified Data**)
25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio..
Viscosity 349000 cP

@Shear Rate 500 1/s,
Temperature 250 °C
349000 cP

@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers