Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 345000 cP @Shear Rate 500 1/s, Temperature 230 °C |
345000 cP @Shear Rate 500 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |