Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 157000 cP @Shear Rate 5000 1/s, Temperature 200 °C |
157000 cP @Shear Rate 5000 1/s, Temperature 392 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Viscosity | 157000 cP @Shear Rate 5000 1/s, Temperature 260 °C |
157000 cP @Shear Rate 5000 1/s, Temperature 500 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Viscosity | 157000 cP @Shear Rate 1450 1/s, Temperature 305 °C |
157000 cP @Shear Rate 1450 1/s, Temperature 581 °F |
ISO 11443 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |