Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 83000 cP @Shear Rate 5000 1/s, Temperature 205 °C |
83000 cP @Shear Rate 5000 1/s, Temperature 401 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Viscosity | 83000 cP @Shear Rate 5000 1/s, Temperature 295 °C |
83000 cP @Shear Rate 5000 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Viscosity | 83000 cP @Shear Rate 5000 1/s, Temperature 240 °C |
83000 cP @Shear Rate 5000 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |