Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 220 cP @Shear Rate 10.0 1/s, Temperature 290 °C |
220 cP @Shear Rate 10.0 1/s, Temperature 554 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Viscosity | 220 cP @Shear Rate 10.0 1/s, Temperature 280 °C |
220 cP @Shear Rate 10.0 1/s, Temperature 536 °F |
|
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Viscosity | 220 cP @Shear Rate 100 1/s, Temperature 270 °C |
220 cP @Shear Rate 100 1/s, Temperature 518 °F |
|
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Viscosity | 220 cP @Shear Rate 1000 1/s, Temperature 270 °C |
220 cP @Shear Rate 1000 1/s, Temperature 518 °F |
|
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |
|||
Viscosity | 220 cP @Temperature 60.0 °C |
220 cP @Temperature 140 °F |
|
BASF Pluracol® TP 4542 Specialty Polyol Description: Pluracol® TPE 4542 polyol is a moderately high molecular weight polyether triol that can be used in polyurethane sealant applications, flexible integral skin foam and cold-cured foam a.. |