Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 135000 cP @Temperature 25.0 °C |
135000 cP @Temperature 77.0 °F |
at 2 rpm vibration |
Permabond F202 Anaerobic Retainer The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a.. |
|||
Viscosity | 135000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
135000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Viscosity | 135000 cP @Frequency 100 Hz, Temperature 292 °C |
135000 cP @Frequency 100 Hz, Temperature 558 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |