Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 110000 - 125000 cP @Temperature 25.0 °C |
110000 - 125000 cP @Temperature 77.0 °F |
at 2.5 rpm vibration |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Viscosity | 110000 cP @Shear Rate 300 1/s, Temperature 190 °C |
110000 cP @Shear Rate 300 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2517 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and low temperature properties with excellent f.. |
|||
Viscosity | 110000 cP @Shear Rate 1000 1/s, Temperature 190 °C |
110000 cP @Shear Rate 1000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow HDPE 25455N High Density Polyethylene DOW HDPE 25455N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and gloss with excellent toughness. This resin has good processability over a.. |
|||
Viscosity | 110000 cP @Shear Rate 100 1/s, Temperature 310 °C |
110000 cP @Shear Rate 100 1/s, Temperature 590 °F |
|
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
Viscosity | 110000 cP @Shear Rate 3090 1/s, Temperature 305 °C |
110000 cP @Shear Rate 3090 1/s, Temperature 581 °F |
ISO 11443 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Viscosity | 110000 cP @Frequency 10.0 Hz, Temperature 322 °C |
110000 cP @Frequency 10.0 Hz, Temperature 612 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Viscosity | 110000 - 4.11e+6 cP @Temperature 275 - 305 °C |
110000 - 4.11e+6 cP @Temperature 527 - 581 °F |
Average value: 999000 cP Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Viscosity | 110000 - 4.11e+6 cP @Shear Rate 7.30 - 3090 1/s |
110000 - 4.11e+6 cP @Shear Rate 7.30 - 3090 1/s |
Average value: 999000 cP Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |