Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 102000 - 458000 cP @Temperature 190 - 200 °C |
102000 - 458000 cP @Temperature 374 - 392 °F |
Average value: 277000 cP Grade Count:29 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Viscosity | 102000 - 458000 cP @Shear Rate 206 - 300 1/s |
102000 - 458000 cP @Shear Rate 206 - 300 1/s |
Average value: 277000 cP Grade Count:29 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Viscosity | 102000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
102000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Viscosity | 102000 cP @Shear Rate 5000 1/s, Temperature 215 °C |
102000 cP @Shear Rate 5000 1/s, Temperature 419 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |
|||
Viscosity | 102000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
102000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |