Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ExxonMobil 20 Exxon XD-3 Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | |
ExxonMobil Mobil Clean 5W-20 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ExxonMobil Univis N 46 UNIVIS N hydraulic oils are high-performance anti-wear fluids designed to meet the needs of all major manufacturers and users of hydraulic equipment. They feature high viscosity indexes (VIs), obtai.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ExxonMobil Teresstic 68 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | Base Oil |
ConocoPhillips Trolley Wire Lube Description: Conoco Trolley Wire Lube is a high-quality, semifluid, lithium-base grease specifically developed for the lubrication of mine trolley wires and shoes. With proper maintenance and freque.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | Base Oil; ASTM D445 |
Chesterton 630 SXCF Synthetic, Extreme Pressure & Corrosion Resistant Grease Description: Superior resistance to washout by water, caustics, sanitizing cleaners, process fluids and steam has now been combined with high temperature performance to product Chesterton® 630 SXCF.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | |
ChevronTexaco Capella® P 68 Texaco Capella P 68 delivers value through:Reduced oil carryover — Low volatility and greater ammonia immiscibility result in significantly less oil reaching the evaporator, increasing refrigeratio.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ELM® SoyLube® All Purpose Lubricant and Penetrating Oil Description: SoyLube All Purpose Lubricant and Penetrating Oil is a high performance, biodegradable penetrant and lubricating oil for general purpose use. Formulated with the best optimized USA-gro.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ChevronTexaco FM ISO 68 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ChevronTexaco ISO 68 Ammonia Refrigeration Oil FeaturesChevron Ammonia Refrigeration Oil provides superior wear protection for reciprocating, vane, and screw compressors.Chevron Ammonia Refrigeration Oil, formulated with ISOSYN® base stocks, is.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | |
ChevronTexaco Rando® HD 68 Ashless Texaco Rando HD Ashless oils deliver value through:Premium performance — Ashless formulation meets or exceeds pump manufacturer requirements for viscosity, rust and corrosion protection, hydrolytic.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ExxonMobil 20 Exxon XD-3 Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | |
ExxonMobil Mobil Clean 5W-20 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ExxonMobil Nuto 68 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ExxonMobil Teresstic 68 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ExxonMobil Univis N 46 UNIVIS N hydraulic oils are high-performance anti-wear fluids designed to meet the needs of all major manufacturers and users of hydraulic equipment. They feature high viscosity indexes (VIs), obtai.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | |
ConocoPhillips Hydroclear Diamond Class® 68 Rotary Compressor Fluid Description: Conoco Hydroclear Diamond Class Rotary Compressor Fluids are designed to lubricate rotary screw compressors operating in air compression service. These semisynthetic products combine hi.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | |
ConocoPhillips Hydroclear® 5W-20 Super All Season and Super Motor Oil Description: Conoco Hydroclear Super All Season Motor Oil SAE 5W-20 is a premium-quality passenger car motor oil developed to meet the requirements of newer, low-friction gasoline engines designed t.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ChevronTexaco Clarity® ISO 68 Hydraulic Oil AW FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | |
ChevronTexaco Cygnus® 68 Hydraulic Oil Texaco Cygnus Hydraulic Oils deliver value through:High quality control — Enables customer to use lubricants almost as pure as the food being processedHigh performance — Provides lubrication bette.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ChevronTexaco GST® ISO 68 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |
|||
Kinematic Viscosity at 100°C (212°F) | 8.5 cSt | 8.5 cSt | ASTM D445 |
ExxonMobil Nuto 68 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |