Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | |
ChevronTexaco Rando® HD 46 Ashless Texaco Rando HD Ashless oils deliver value through:Premium performance — Ashless formulation meets or exceeds pump manufacturer requirements for viscosity, rust and corrosion protection, hydrolytic.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | ASTM D445 |
ExxonMobil 798 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | |
ConocoPhillips 46 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | |
ConocoPhillips Hydroclear Diamond Class® 46 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | |
ConocoPhillips Hydroclear Diamond Class® 46 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | |
ConocoPhillips Hydroclear® 46 Refrigerant Oil Description: Conoco Hydroclear Refrigerant Oil is a high-quality ammonia refrigeration compressor lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Refrigerant Oil is spe.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | ASTM D445 |
ChevronTexaco Clarity® ISO 46 Hydraulic Oil AW FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | |
ConocoPhillips 46 Ultra-Clean Super Hydraulic Oil Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | |
ConocoPhillips HD Fleet™ 10W Engine Oil Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | |
ConocoPhillips Hydroclear® 46 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | ASTM D445 |
ExxonMobil 46 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® SAE 20 White Mineral Oil Food Grade Trolley Oil ISO 46 Description: ANDEROL PQ Trolley Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ Trolley Oil is recomm.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | ASTM D445 |
ExxonMobil 46 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.8 cSt | 6.8 cSt | ASTM D445 |
ExxonMobil 798 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |