ConocoPhillips Hydroclear® 46 AW Hydraulic Fluid

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® 46 AW Hydraulic Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard antiwear hydraulic fluids. Hydroclear AW Hydraulic Fluid is specially formulated with proprietary additive chemistry and Conoco hydrocracked base oils. Hydroclear AW Hydraulic Fluid is recommended for use in a variety of high-pressure mobile and stationary hydraulic systems utilizing vane, piston or gear pumps. Hydroclear AW Hydraulic Fluid has been tested and approved by Denison Hydraulics in accordance with its premium HF-0 requirements. Hydroclear AW Hydraulic Fluid significantly exceeds the requirements of and has been formally approved by Cincinnati Milacron under specifications P-68 (ISO 32), P-70 (46) and P-69 (68). Hydroclear AW Hydraulic Fluid exceeds Vickers M-2950-S, Vickers I-286-S and U.S. Steel 127 and 136 requirements. Hydroclear AW Hydraulic Fluid MV is available in several grades formulated with exceptional shear stable additives. Hydroclear AW Hydraulic Fluid MV grades are high-viscosity index products with exceptionally low pour points and superior low-temperature pumpability. Hydroclear AW Hydraulic Fluid MV grades can be used year-round in hydraulic systems in virtually all climates.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.866 g/cc
0.0313 lb/in³
Viscosity Measurement 100
100
Viscosity Index
Saybolt Viscosity at 100°F 237 SUS
237 SUS
Saybolt Viscosity at 210°F 49 SUS
49 SUS
Kinematic Viscosity at 40°C (104°F) 46 cSt
46 cSt
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
Oxidative Stability 7500 hour
7500 hour
ASTM D 943
ASTM Color 0.50
0.50
Mechanical Properties Metric English Comments
Four Ball Wear 0.400 mm
0.0157 in
Thermal Properties Metric English Comments
Pour Point -34.4 °C
-30.0 °F
Flash Point 232 °C
450 °F
Electrical Properties Metric English Comments
Dielectric Strength 40.0 kV/mm
1020 kV/in
No thickness given
Descriptive Properties Value Comments
Emulsion Characteristics (40-40-0) 10 minutes
FZG Pass 12