Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 23 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 32 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 320 Mobil DTE PM Ashless
Mobil DTE PM Ashless products are high-performance, environmentally friendly lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provi..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 320 Mobil DTE PM Series
Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Enmist EP 320
Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist ..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil CM-P Mobilgrease CM Series
Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Centaur Moly 1
Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly  products represents a sign..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Centaur Moly 2
Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly  products represents a sign..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Spartan EP 320
Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Teresstic 320
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Delvac Xtreme Service Grease
Mobil Delvac Xtreme Service Grease is an extra high performance extreme-pressure grease. It is an NLGI 2 grade and is manufactured with a proprietary, high-temperature lithium complex thickener syst..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Vaculine 137
The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
See Note 3.
ChevronTexaco Starplex® Moly MPGM 2
Texaco Starplex Moly MPGM grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending ..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
See Note 3.
ChevronTexaco Starplex® Moly NLGI Grade 1
Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 32 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 320 Mobil DTE PM Ashless
Mobil DTE PM Ashless products are high-performance, environmentally friendly lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provi..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 320 Mobil DTE PM Series
Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 320 Mobilgear SHC Series
The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 632 Mobilgear 600 Series
The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives ..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Enmist EP 320
Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist ..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Centaur Moly 2
Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly  products represents a sign..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Glygoyle 320
Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Vaculine 137
The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Spartan EP 320
Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
See Note 3.
ChevronTexaco Starplex® Moly NLGI Grade 2
Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil 23 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Delvac Xtreme Service Grease
Mobil Delvac Xtreme Service Grease is an extra high performance extreme-pressure grease. It is an NLGI 2 grade and is manufactured with a proprietary, high-temperature lithium complex thickener syst..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Almo 532
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil CM-S Mobilgrease CM Series
Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ..
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
ExxonMobil Mobil Almo 532
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..