Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | Base Oil; ASTM D445 |
Nye Lubricants 571H-10 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8920U (491UV) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 3 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 629 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil Enmist EP 150 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil Ronex MP Exxon RONEX MP is a premium quality multipurpose grease that can be used in a wide range of automotive and industrial applications. RONEX MP consists of a mineral oil base fluid thickened with a lit.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 150 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ChevronTexaco 940 Gas Engine Oil Chevron Gas Engine Oil 940 is a medium ash, intermediate base number, dispersant/detergent type engine oil.It is manufactured using highly refined paraffinic base oils and an additive package contai.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ChevronTexaco Delo® 194 Marine Engine Oil, SAE 40 Chevron Marine Engine Oil Delo 194 is a high quality, low ash oil formulated to meet the requirements of the great majority of high speed marine diesel engine manufacturers.It is manufactured using .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | |
ChevronTexaco URSA® SAE 40 Super Plus Texaco Ursa Super Plus oils deliver value through:Oil lasts longer between drains — Good oxidation stability protects against oil thickening during manufacturers recommended oil drain periods.Vital.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 150 Mobil DTE PM Ashless Mobil DTE PM Ashless products are high-performance, environmentally friendly lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provi.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 150 Mobil DTE PM Series Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 150 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 150 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 19M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 3 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil CM-L Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil CM-W Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil Enmist EP 150 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 128 The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil Mobilith AW Series 0 The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® AA-40 White Mineral Food Grade Oil, ISO Grade 150, SAE Grade 40 Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | |
ConocoPhillips Hydroclear® 150 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 1 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil Mobil Glygoyle 150 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil CM-W Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ChevronTexaco Rykon® NLGI 1 Premium Grease EP FeaturesChevron Rykon Premium Grease EP is a high quality, water resistant, extreme pressure, multipurpose lubricating grease.It is manufactured using highly refined, select high viscosity index bas.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | |
ConocoPhillips 150 Bearing Oil Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi.. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil 19M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Kinematic Viscosity at 40°C (104°F) | 150 cSt | 150 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 128 The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti.. |