Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 162 cSt | 162 cSt | |
Lubriplate AC-4 Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 162 cSt | 162 cSt | |
Lubriplate H0-4 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Kinematic Viscosity at 40°C (104°F) | 162 cSt | 162 cSt | |
Lubriplate SYN LUBE 150 PAO-Based Multi-Purpose Synthetic Fluid PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 150, 220, 320, 460 & 680 are recommended.. |
|||
Kinematic Viscosity at 40°C (104°F) | 162 cSt | 162 cSt | |
Lubriplate NO.4 Petroleum-Based Machine Tool Oil Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles.. |