Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.41 - 1.43 g/cc | 1.41 - 1.43 g/cc | ISO.1183 DN.53479 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D792 |
S&E Specialty Polymers GA-1021-CJ PVC Application: 75° C CMR, CL2R, AND FPLR flame retardant jacketing compound.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina 801-08/98-C-IS Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina 801-10/49-C-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina 801-10/88-CR White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina 804-02/69-Y-RTC Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina 811-18/466-Y-CRB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | NBR 14288 |
Karina 850-10/179-Y-ERYM-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of window profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina 850-10/199-Y-ERYM White PVC Compound White PVC compound recommended for windows and profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina CAK 35-F Ivory PVC Compound Reclaimed PVC compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina CAK 751-48/1-TEC-IS Black PVC Compound Reclaimed PVC compound, recommended for plug injection.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 828-08/497-Y-RT Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 828-18/569-Y-RT Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 839-10/68-Y-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 850-35/1-C Ivory PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 854-10/144-ERYM White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 857-35/1-A-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom PT-109599 PVC Description: Polycom rigid PVC compounds for the extrusion of pipes have excellent processing characteristics and are available in the form of pellets and dry blend. They are available with lead and.. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 8553 Moldings & Extrusions Flexible PVC A general purpose profile extrusion compound with excellent weathering properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 13820 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications. Good low temperature performance. Also suitable for outdoor jacket applicatio.. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 13821 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gul.. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 14910 Wire & Cable Flexible PVC Flame retardant jacket compound recommended for CM, CL2 type constructions when used over FR-PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 38900 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 898 Wire & Cable Flexible PVC Non-lead stabilized, flame retardant, non-migratory, 105°C insulation compound recommended for use in non-migratory applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo.. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 28930 Coax & Telecom Flexible PVC Non-lead stabilized 105C FT-4 riser jacket compound. UV resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 4890 Flexible PVC Non-lead stabilized, 85C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 06/148-GE Blue Color Concentrate for PVC Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 837-10/68-Y-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |