Specific Gravity 3.70 g/cc
3.70 g/cc
ASTM D792
Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene
Nontoxic alternative to Lead (Pb), for shielding applicationsHigh Specific GravityCarbonyl Iron Filled Polypropylene Random Co-PolymerInformation provided by Technical Polymers
Specific Gravity 3.70 g/cc
3.70 g/cc
silicone property; Arlon SQA-TMS-024
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Specific Gravity 3.70 g/cc
3.70 g/cc
silicone property; Arlon SQA-TMS-024
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.