Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.875 - 3.125 g/cc | 1.875 - 3.125 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by .. |
|||
Specific Gravity | 1.875 g/cc @Temperature 20.0 °C |
1.875 g/cc @Temperature 68.0 °F |
|
Indium Corp. Germanium Corporation® GeCl4 Germanium Tetrachloride Germanium tetrachloride is a colorless liquid. It is used as an intermediate in the production of purified germanium dioxide and germanium metal, but more predominantly used as a reagent in fiber o.. |