Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.37 g/cc | 1.37 g/cc | Part A; TM R050-16 |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable W1200 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
PlastiComp Complet® LCF50-PA66 50% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D-792 |
PlastiComp Velocity® LCF50-PA66 High Flow Nylon 66, 50% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D 792 |
SABIC Innovative Plastics Extem UH1016M TPI Blend High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D 792 |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
Specific Gravity | 1.37 - 1.43 g/cc | 1.37 - 1.43 g/cc | ASTM D 792 |
Karina E 901-48/1-F-ISM Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Fiberfil® FV-31 Nylon 6, 31% Glass Reinforced, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7023/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | Absolute Drying; ASTM-D792 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D790 |
Clariant Renol 66G33HSL Nylon 66, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Clariant Renol PA111G35IF Nylon 66, 35% Glass Fiber, Improved Flow Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.37 - 1.41 g/cc | 1.37 - 1.41 g/cc | ASTM D-792 |
Axiall 8621 Moldings & Extrusions Flexible PVC High quality, semi-rigid extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia .. |
|||
Specific Gravity | 1.37 - 1.41 g/cc | 1.37 - 1.41 g/cc | ASTM D-792 |
Axiall 17881 Wire & Cable Flexible PVC THW insulation compound. UL recognized component for TW, THW insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | Part A; TM R050-16 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ISO 1183 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ISO 1183 |
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ISO 1183 |
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |