Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP 307 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
PolyOne Maxxam™ NT-818.B001-7001 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | |
Northstar Polymers APX-005 Curing Agent Information provided by Northstar Polymers. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | |
Resinlab® RC8038 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Specific Gravity | 1.02 - 1.04 g/cc | 1.02 - 1.04 g/cc | |
Michelman® Plate Kote™ 42S KOSHER Water based OPV Description: Water based OPV for paper platesUsage: Plate Kote™ 42S is a food-contact compliant release coating which has been formulated solely for the unique requirements of paper plate conve.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL SA90 PPE (Asia Pacific) Noryl* SA90 resin is a modified low molecular weight resin with increased hydroxyl functionality. It is designed specifically for use as a reactive component in epoxy and cyanate ester thermosets i.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL SA9000 PPE (Europe-Africa-Middle East) Noryl* SA9000 resin is a modified low molecular weight resin with vinyl end-groups. It is well suited for use with other unsaturated monomers and resins which cure via free radical reactions. These .. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCD795 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SVE and NISPE confiations. Flame retardant performance capable of m.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | |
Shin-Etsu Silicones KE-109A/B Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Teknor Apex Synres® PP G20 62 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | |
Teknor Apex Tekbond® TB 2005 Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1431B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1434A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-2503S Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 30424 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 30424 is a green color concentrate based in polyethylene. This concentrate was designed to provide color in blow molding and injection molding applications. POLYBATCH® 3042.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | |
Zeon Chemicals Nipol® DN003 Nitrile Elastomer Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is .. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ISO 1183 |
Total PS CPDS 9217 Compound Polystyrene/Polyethylene POLYSTYRENE (PS) COMPOUND (CPDS) 9217 is an alloy of polystyrene and polyethylene. This combination brings the benefits of polyethylene; a high level of stress crack resistance, mechanical properti.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ISO 1183 |
Ter Hell Plastic K-Resin KRE 9902 Butadiene-Styrene Copolymer Description: Butadiene-Styrene Copolymer Compound, good transparency with impact strength and stiffness well-balanced.Application: For all kinds of injection molded parts.Information provided by T.. |
|||
Specific Gravity | 1.02 g/cc @Temperature 25.0 °C |
1.02 g/cc @Temperature 77.0 °F |
|
Dow Corning 806A RESIN Silicone binder resin for colored baking enamels for space heaters, stoves, etc. Used alone or blended with Dow Corning® 805 Resin to promote intermediate hardness.Information provided by Dow Corni.. |
|||
Specific Gravity | 1.02 g/cc @Temperature 25.0 °C |
1.02 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7780 RELEASE MODIFIER Syl-off® 7780 Release Modifier is a 100% active solids, pre-catalysed, release modifier. High efficiency release modifier suitable for use with Syl-off® brand silicone release coatings.Information.. |
|||
Specific Gravity | 1.02 g/cc @Temperature 25.0 °C |
1.02 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7791 RELEASE MODIFIER Syl-Off® 7791 Release Modifier is a 100% active solids release modifier. A High efficiency release modifier suitable for use with Syl-Off® 7040 Coating.Information provided by Dow Corning |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | |
Chesterton OPTICOOL™ 575 Lubrication Description: OPTICOOL 575 is a high performance blend of synthetic and emulsion technology, OPTICOOL 575 formulation offers superior lubrication/cooling, corrosion inhibition, extreme pressure resis.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | Part B |
Epoxy Technology EPO-TEK® 330 Low Viscosity, Optical Epoxy Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications.Advan.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | Part B |
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | Part B |
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Asahi Kasei Thermylene® P6-16FG-0801 16% Fiber Glass Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | "A" component |
ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating QLE 1101 is a low viscosity, two-component, addition cure, silicone elastomer.Key Features: Fast cure at elevated temperaturesLow linear shrinkageTransparent, ideal for pigmentationLow viscosity Par.. |