Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.941 g/cc | 0.941 g/cc | ISO 1183 |
Polimeri Europa Greenflex® FF 55 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 55 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 55 show high flexibility.Main Applications: Greenflex FF 55 is recommended f.. |
|||
Specific Gravity | 0.941 g/cc | 0.941 g/cc | ISO 1183 |
Polimeri Europa Greenflex® ML 50 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion Greenflex ML 50 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 50 show high elasticity.Main Applications: Greenflex.. |
|||
Specific Gravity | 0.941 g/cc | 0.941 g/cc | ISO 1183 |
Polimeri Europa Greenflex® MQ 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MQ 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MQ 40 combines high fluidity and high elasticity.Main Applications: Green.. |
|||
Specific Gravity | 0.941 g/cc | 0.941 g/cc | 20/20°C |
LyondellBasell Glycol Ether EBA Ethylene glycol butyl ether acetate Information provided by Lyondell. |
|||
Specific Gravity | 0.941 g/cc | 0.941 g/cc | ISO 1183 |
Polimeri Europa Clearflex® RL 50 U Linear Medium Density Polyethylene Clearflex RL 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |