Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.78 g/cc | 7.78 g/cc | |
Latrobe Lescowearâ„¢ Cold Work Tool Steel Lescowear cold work tool steel is a versatile medium-chromium, air-hardening tool steel that is characterized by a very good combination of toughness and wear resistance. It is available primarily i.. |
|||
Specific Gravity | 7.78 g/cc | 7.78 g/cc | |
Latrobe LSSâ„¢ A9 Tool Steel (ASTM A9) TLS A9 tool steel is a 5% chromium tool steel with a unique combination of properties which make it suitable for both cold work and hot work tooling applications. The combination of nickel, vanadium.. |
|||
Specific Gravity | 7.78 g/cc | 7.78 g/cc | |
Latrobe LSSâ„¢ H10 Hot Work Tool Steel (ASTM H10) TLS H10 hot work tool steel is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is very resistant to thermal fatigue cracking .. |
|||
Specific Gravity | 7.78 g/cc | 7.78 g/cc | |
Latrobe 14-4CrMo Stainless Tool Steel 14-4CrMo is a wear resistant, martensitic stainless tool steel that exhibits better corrosion resistance than Type 440C stainless steel. The molybdenum in the steel provides superior corrosion resis.. |
|||
Specific Gravity | 7.78 g/cc | 7.78 g/cc | |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
Specific Gravity | 7.78 g/cc | 7.78 g/cc | |
Latrobe LSS™ MGR™ Tool Steel (ASTM A8) TLS MGR tool steel is an air-hardening tool steel that is characterized by a combination of very good toughness, intermediate wear resistance, and excellent dimensional stability in heat treatment. .. |