Specific Gravity 3.045 - 3.955 g/cc
3.045 - 3.955 g/cc
ASTM D792
Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer
Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s..
Specific Gravity 3.045 - 3.955 g/cc
3.045 - 3.955 g/cc
ASTM D792
Parker Chomerics Tecknit Consil®-C 873 Silver-Copper Filled Silicone Elastomer
Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s..
Specific Gravity 3.045 - 3.955 g/cc
3.045 - 3.955 g/cc
ASTM D792
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-RHT 855 is a pure silver-filled silicone elastomer ideal for applications where high temperature is a concernTypical Applications: CONSIL-RHT 855 silicone is used throughout indu..
Specific Gravity 3.045 - 3.955 g/cc
3.045 - 3.955 g/cc
ASTM D792
Parker Chomerics Waveguide Gaskets 873 Conductive Silicone Elastomer Gasket
Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W..
Copyright © lookpolymers.com All Rights Reserved